Problem 1
Aluminum exhibits a Face-Centered Cubic (FCC) crystal lattice structure with a unit cell lattice parameter of $a = 0.4050\text{ nm} = 4.050 \times 10^{-10}\text{ m}$. What is the planar atomic density $PD_{(111)}$ on the close-packed $(111)$ crystallographic plane in atoms per square nanometer ($\text{atoms/nm}^2$)? Enter your answer rounded to one decimal place (e.g., 14.1).
Show the solution
**Step 1: Determine Atoms in the (111) Plane Triangle** From the FE Reference Handbook (Materials Science / Crystallography / Planar Density): In an FCC unit cell, the $(111)$ plane intersects the cube diagonals forming an equilateral triangle whose sides equal the face diagonal: $$s = a\sqrt{2} = (0.4050\text{ nm})\sqrt{2} = 0.572756\text{ nm}$$ The planar triangle encloses: - 3 corner atoms, each shared among 6 adjacent triangles: $3 \times (1/6) = 0.5\text{ atoms}$ - 3 edge-centered face atoms, each shared between 2 triangles: $3 \times (1/2) = 1.5\text{ atoms}$ Total effective atoms centered on the plane: $$N_{atoms} = 0.5 + 1.5 = 2.0\text{ atoms}$$ **Step 2: Calculate Area of (111) Triangular Plane** $$A_{(111)} = \frac{\sqrt{3}}{4} s^2 = \frac{\sqrt{3}}{4} (a\sqrt{2})^2 = \frac{\sqrt{3}}{2} a^2$$ $$A_{(111)} = \frac{\sqrt{3}}{2} (0.4050\text{ nm})^2 = 0.866025 \times 0.164025 = 0.142049\text{ nm}^2$$ **Step 3: Compute Planar Density $PD_{(111)}$** $$PD_{(111)} = \frac{N_{atoms}}{A_{(111)}} = \frac{2.0\text{ atoms}}{0.142049\text{ nm}^2} = 14.0797\text{ atoms/nm}^2 \approx 14.1\text{ atoms/nm}^2$$ Conclusion: The planar atomic density is **$14.1\text{ atoms/nm}^2$**.
Problem 2
Which **TWO** of the following statements regarding the heat treatment, microstructural phase transformations, and mechanical property evolution of plain carbon steels are **TRUE**?
- ARapid water or brine quenching of austenite to room temperature produces a hard, brittle, body-centered tetragonal (BCT) non-equilibrium phase called martensite via a diffusionless shear transformation.
- BFull annealing consists of rapid quenching from the austenite region followed by sub-critical cryogenic cooling to eliminate all residual ductility.
- CTempering a quenched steel involves reheating it below the lower eutectoid temperature (A1) to precipitate fine iron carbides (Fe3C), significantly enhancing toughness and impact resistance at the expense of peak hardness.
- DPearlite consists of a single homogeneous solid-solution crystalline phase devoid of any lamellar boundary interfaces.
Show the solution
Evaluation of heat treatment and phase transformation principles: 1. Statement A (TRUE): Martensitic transformation is an athermal, diffusionless, military-style shear displacement of iron atoms. When austenite (FCC) is cooled below the martensite start ($M_s$) temperature at rates exceeding the critical cooling rate, carbon atoms cannot diffuse out to form cementite. Instead, they remain interstitial, distorting the iron unit cell into body-centered tetragonal (BCT) martensite, which is characterized by extremely high hardness and brittleness. 2. Statement B (FALSE): Full annealing involves heating hypoeutectoid steel into the austenite phase field, followed by very slow, controlled furnace cooling. The goal of annealing is to produce coarse pearlite and proeutectoid ferrite, resulting in minimum hardness, maximum ductility, and complete relief of internal residual stresses. 3. Statement C (TRUE): Tempering is a sub-critical thermal process applied to as-quenched martensite. Reheating between $200^\circ\text{C}$ and $650^\circ\text{C}$ provides sufficient thermal energy for trapped carbon to precipitate as extremely fine, dispersed cementite ($\text{Fe}_3\text{C}$) particles embedded within a ductile ferrite matrix. This transforms brittle martensite into tempered martensite, restoring toughness and impact resistance. 4. Statement D (FALSE): Pearlite is not a single phase; it is a two-phase lamellar microconstituent formed by the eutectoid decomposition of austenite at $727^\circ\text{C}$ ($0.77\text{ wt\% C}$): $$\gamma (0.77\text{ wt\% C}) \longrightarrow \alpha (0.022\text{ wt\% C}) + \text{Fe}_3\text{C} (6.70\text{ wt\% C})$$ It consists of alternating thin plates (lamellae) of soft, ductile ferrite ($\alpha$) and hard, brittle cementite ($\text{Fe}_3\text{C}$). Therefore, the two correct statements are A and C.
Problem 3
In physical metallurgy and mechanical behavior of crystalline materials, crystal lattice structures dictate deformation mechanisms and brittle-ductile transition behavior. Which of the following statements correctly describe metallic crystal structures and their deformation characteristics? Select the TWO correct statements:
- AFace-Centered Cubic (FCC) metals (such as copper, aluminum, and austenitic stainless steel) maintain high ductility even at cryogenic temperatures because they possess 12 close-packed slip systems ({111} ) and do not exhibit a distinct ductile-to-brittle transition temperature (DBTT).
- BBody-Centered Cubic (BCC) metals (such as ferritic iron, tungsten, and chromium) exhibit a pronounced ductile-to-brittle transition temperature (DBTT) because dislocation Peierls barrier resistance increases significantly as temperature decreases.
- CHexagonal Close-Packed (HCP) metals exhibit the highest room-temperature ductility of all metallic systems because they contain 48 independent intersecting slip systems.
- DFace-Centered Cubic (FCC) crystals have an atomic packing factor (APF) of 0.68, which is lower than that of Body-Centered Cubic (BCC) crystals.
Show the solution
Step 1 - Crystal Slip Systems and Ductility: 1. Face-Centered Cubic (FCC): - Contains 4 {111} close-packed planes with 3 directions each = 12 independent close-packed slip systems. - Dislocations move readily even at liquid nitrogen temperatures; FCC metals do NOT exhibit a ductile-to-brittle transition temperature (DBTT). -> Option A is TRUE. 2. Body-Centered Cubic (BCC): - Lacks truly close-packed planes; slip occurs on {110}, {112}, and {123} planes. - Peierls stress (lattice friction resisting dislocation motion) is strongly thermally activated. - At sub-ambient temperatures, dislocation glide freezes, triggering cleavage fracture (pronounced DBTT). -> Option B is TRUE. Step 2 - Analyze Distractors C and D: - Option C: HCP metals (e.g., zinc, magnesium, titanium) have restricted slip systems (only 3 in the basal plane at room temperature) and typically exhibit low ductility and high anisotropy. - Option D: FCC has an atomic packing factor (APF) of 0.74 (close-packed), while BCC has an APF of 0.68 (non-close-packed). Correct selection: ["A","B"].