A 316L stainless steel agitator shaft operating in a chemical reaction medium containing chloride ions undergoes uniform electrochemical corrosion. An electrochemical polarization test gives a measured corrosion current density of $i_{corr} = 15.0\text{ }\mu\text{A/cm}^2$. The alloy has an equivalent weight of $EW = 25.5\text{ g/equivalent}$ and a density of $\rho = 8.00\text{ g/cm}^3$. Using Faraday's law of electrolysis as formulated in the FE Reference Handbook, the Corrosion Penetration Rate (CPR) in millimeters per year is most nearly:
- A0.085 mm/yr
- B0.156 mm/yrcorrect
- C0.245 mm/yr
- D0.382 mm/yr
Show the solution
Step 1: Identify the Corrosion Penetration Rate (CPR) equation from the FE Reference Handbook: $$CPR = K \dfrac{i_{corr} \cdot EW}{\rho}$$ where the metric conversion constant is $K = 0.00327\text{ mm}\cdot\text{g}/(\mu\text{A}\cdot\text{cm}\cdot\text{yr})$ when $i_{corr}$ is in $\mu\text{A/cm}^2$, $EW$ is in g/equiv, and $\rho$ is in $\text{g/cm}^3$. Step 2: Substitute the known values: $$i_{corr} = 15.0\text{ }\mu\text{A/cm}^2$$ $$EW = 25.5\text{ g/equivalent}$$ $$\rho = 8.00\text{ g/cm}^3$$ Step 3: Calculate the corrosion rate: $$CPR = 0.00327 \times \dfrac{15.0 \times 25.5}{8.00} = 0.00327 \times \dfrac{382.5}{8.00} = 0.00327 \times 47.8125$$ $$CPR = 0.15635\text{ mm/year} \approx 0.156\text{ mm/yr}$$ Step 4: Engineering significance: With an annual loss of $0.156\text{ mm/yr}$, a standard corrosion allowance of $2.0\text{ mm}$ will protect the equipment for $2.0 / 0.156 = 12.8\text{ years}$. Distractor Analysis: - Option A (0.085 mm/yr) uses the molar mass of iron ($55.85$) instead of the equivalent weight divided by valence. - Option C (0.245 mm/yr) uses density of titanium or aluminum instead of steel ($8.0\text{ g/cm}^3$). - Option D (0.382 mm/yr) forgets the conversion factor $K$ or divides incorrectly by $\rho$.